Adnyana, D. N. (2017) “Korosi Retak Tegang pada Pipa Superheater Ketel Uap yang Baru Dibangun [Stress Corrosion Cracking of Cage Superheater Tubes of a Newly Built Boiler]”, Jurnal Metalurgi, 32(3), pp. 123–136. doi: 10.14203/metalurgi.v32i3.357.